Abstract. The addition of small amounts (up to 9wt%) of chitin microsized particles, originating from shellfish waste, tocarboxylated styrene-butadiene rubber (XSBR) matrix (as received and annealed to 100°C) has been studied. In particular,this study concentrated on their mechanical (creep investigation by nanoindentation and dynamical-mechanical analysis),thermal (differential scanning calorimetry and thermogravimetry) and swelling behaviour (toluene absorption) and wascompleted by morphological characterisation by scanning electron microscopy and atomic force microscopy.The results show that annealing has a limited effect on materials properties, effects which are further reduced by the addi-tion of growing amounts of crab chitin. It should be noted that the limited filler content used in the study does not substan-tially modify the linear creep behaviour of XSBR for sufficiently long loading times. The thermal stability of the systemdoes also appear to be preserved even with the maximum chitin content added, while it serves sufficiently as an effective barrier against aromatic solvent absorption.

Mechanical and thermal properties of crab chitin reinforced carboxylated SBR composites

MONTI, MARCO;PUGLIA, Debora;RALLINI, MARCO;KENNY, Jose Maria
2012

Abstract

Abstract. The addition of small amounts (up to 9wt%) of chitin microsized particles, originating from shellfish waste, tocarboxylated styrene-butadiene rubber (XSBR) matrix (as received and annealed to 100°C) has been studied. In particular,this study concentrated on their mechanical (creep investigation by nanoindentation and dynamical-mechanical analysis),thermal (differential scanning calorimetry and thermogravimetry) and swelling behaviour (toluene absorption) and wascompleted by morphological characterisation by scanning electron microscopy and atomic force microscopy.The results show that annealing has a limited effect on materials properties, effects which are further reduced by the addi-tion of growing amounts of crab chitin. It should be noted that the limited filler content used in the study does not substan-tially modify the linear creep behaviour of XSBR for sufficiently long loading times. The thermal stability of the systemdoes also appear to be preserved even with the maximum chitin content added, while it serves sufficiently as an effective barrier against aromatic solvent absorption.
2012
File in questo prodotto:
Non ci sono file associati a questo prodotto.

I documenti in IRIS sono protetti da copyright e tutti i diritti sono riservati, salvo diversa indicazione.

Utilizza questo identificativo per citare o creare un link a questo documento: https://hdl.handle.net/11391/1123869
Citazioni
  • ???jsp.display-item.citation.pmc??? ND
  • Scopus 19
  • ???jsp.display-item.citation.isi??? 15
social impact